<?xml version="1.0" encoding="UTF-8"?><?xml-stylesheet type="text/xsl" href="static/style.xsl"?><OAI-PMH xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/ http://www.openarchives.org/OAI/2.0/OAI-PMH.xsd"><responseDate>2026-11-21T04:13:45Z</responseDate><request verb="GetRecord" identifier="oai:macsphere.mcmaster.ca:11375/19215" metadataPrefix="dim">https://prod-ms-be.lib.mcmaster.ca/server/oai/request</request><GetRecord><record><header><identifier>oai:macsphere.mcmaster.ca:11375/19215</identifier><datestamp>2026-09-24T21:22:04Z</datestamp><setSpec>com_11375_271</setSpec><setSpec>col_11375_272</setSpec></header><metadata><dim:dim xmlns:dim="http://www.dspace.org/xmlns/dspace/dim" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xmlns:doc="http://www.lyncode.com/xoai" xsi:schemaLocation="http://www.dspace.org/xmlns/dspace/dim http://www.dspace.org/schema/dim.xsd">
   <dim:field mdschema="dc" element="contributor" qualifier="advisor">Petric, Anthony</dim:field>
   <dim:field mdschema="dc" element="contributor" qualifier="author">Zou, Yun</dim:field>
   <dim:field mdschema="dc" element="contributor" qualifier="department" lang="en_US">Materials Engineering</dim:field>
   <dim:field mdschema="dc" element="date" qualifier="accessioned">2016-05-05T14:02:06Z</dim:field>
   <dim:field mdschema="dc" element="date" qualifier="available">2016-05-05T14:02:06Z</dim:field>
   <dim:field mdschema="dc" element="date" qualifier="issued">1993-06</dim:field>
   <dim:field mdschema="dc" element="identifier" qualifier="uri">http://hdl.handle.net/11375/19215</dim:field>
   <dim:field mdschema="dc" element="identifier" qualifier="uri">https://doi.org/10.71548/17475</dim:field>
   <dim:field mdschema="dc" element="description" qualifier="abstract" lang="en_US">&lt;p> Ceramic samples of Li2+xYxZr1-xO3 with x=0 to 0. 1, Li8+xYxZr1-xO6 with x=0 to 0.2, Li1-xYxZr1-xO2 with x=0 to 0.5 and Li1+xZrxY1-xO2+x with x=0 to 0. 3 were prepared via conventional solid reactions. The solubilities, crystal structures and microstructures in these samples were studied by x-ray diffraction(XRD), infrared spectra, differential thermal&#xd;
analysis(DTA) and scanning electron microscopy(SEM). The&#xd;
results show that the solubilities are 0.05≤X&lt;0.1 for Li2+xYxZr1-xO3 and Li8+xYxZr1-xO6,  0.1≤x&lt;0.15 for Li1-xYxZr1-xO2, and x≥0.3 for Li1+xZrxY1-xO2+x, respectively. The crystal structures of the solid solutions of Li2+xYxZr1-xO3 and Li8+xYxZr1-xO6 are the same as Li2ZrO3 and Li8ZrO6, respectively but the cell constants change slightly with x, while the structure of Li1-xYxZr1-xO2 and Li1+xZrxY1-xO2+x changes from monoclinic for pure LiYO2 (x=0) to tetragonal (x≥0.005). The sinterability of Li2ZrO3 improves greatly with yttrium additions to Li2ZrO3. &lt;/p> &lt;p> The conductivities of the samples were measured by&#xd;
complex impedance spectroscopy and dc polarization. The results show that lithium conductivity in Li2+xYxZr1-xO3 samples increases slightly from 3.9x10^-6 to 5.0x10^-6 S/cm at 400°C as x increases from 0 to 0.05 and the corresponding conduction activation energy decreases slightly from 0.99 to 0.92 eV. Based on the effective medium theory, the conductivity increase in the solid solution was estimated to be 3% for x=0.05 compared with pure Li2ZrO3 crystal.&lt;/p> &lt;p>For Li8+xYxZr1-xO6 samples, a mixture of LiOH and Li2CO3,&#xd;
which melts at about 430°C, can be formed during the processing and measurements. The ionic conductivity depends to a large degree on the microstructure(the amount and&#xd;
distribution of the mixture) below 430°C. The lithium conductivity at 435°C increases from 1.0x10^-2 to 6.9x10^-2 S/cm as x increases from 0 to 0.05. The electronic contribution to&#xd;
total conductivity is lower than 1% below 435°C.&lt;/p> &lt;p> The ionic conductivity in the tetragonal phase of Zr-doped LiYO2 is much lower than in pure monoclinic LiYO2. The&#xd;
conductivity values at 500°C are 1.3x10^-2 for pure LiYO2 and 1.2x10^-4 for Li1.3Zr0.3Y0.7O2.3. The ionic conduction activation energy in the tetragonal Zr-doped LiYO2 is much higher than pure LiYO2.&lt;/p> &lt;p> The thermal stability and the hydrolysis tendency for Li2ZrO3, Li8ZrO6 and LiYO2 were examined by thermodynamic calculations and by experiments.&lt;/p></dim:field>
   <dim:field mdschema="dc" element="description" qualifier="degreetype" lang="en_US">Thesis</dim:field>
   <dim:field mdschema="dc" element="description" qualifier="degree" lang="en_US">Master of Engineering (MEngr)</dim:field>
   <dim:field mdschema="dc" element="language" qualifier="iso" lang="en_US">en_US</dim:field>
   <dim:field mdschema="dc" element="subject" lang="en_US">structure, properties, lithium, ion, conductors, crystal</dim:field>
   <dim:field mdschema="dc" element="title" lang="en_US">Structure and Properties of Lithium Ion Conductors in the Li2O-Y2O3-ZrO2 System</dim:field>